ARALDITE AV 8503

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE AV 8503

Main features

  • One-Minute Fixturing Time
  • Heat-Resistant Bonding Service
  • 1:1 Controlled Mixing

Product Description

ARALDITE® AV 8503 Resin / Hardener HV 8503 is a two-component epoxy adhesive paste developed for bonding sheet molding compound, plastics, and metals. The blue resin and beige hardener mix at a convenient 1:1 ratio by volume and form a non-sag paste with approximately 100 minutes of pot life at 25°C. The adhesive combines good flexibility with heat resistance and can achieve rapid handling strength using a heated fixture. Its surface-preparation requirements are limited to a dry wipe before bonding, supporting straightforward assembly processes where controlled paste application and accelerated heat cure are required.

Key features

  • Rapid heat fixture: Reaches fixture strength in approximately one minute on a fixture heated to 116°C.
  • Flexible cured epoxy: Provides 15% elongation with a Shore D hardness of 78.
  • Convenient paste mixing: Uses a 1:1 mix ratio by volume with good weldability and non-sag application behavior.

Applications / Suitable for

  • Sheet molding compound bonding
  • Plastic assembly
  • Metal bonding

Technical Specifications

General Properties
Color Color
blue
Pot Life Pot Life
30 minutes
Specific Gravity Specific Gravity
1.32
Physical Properties
Viscosity (Part A) Viscosity (Part A)
172000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
103 °C
Mechanical Properties
Elongation Elongation
15 %