ALPHA WS600

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA WS600

Main features

  • Three Application-Specific Viscosity Options
  • Eight-Hour Stencil Life
  • Water-Soluble Halide-Free Chemistry

Product Description

ALPHA WS-600 Paste Flux Series is a family of completely water-soluble BGA and CSP fluxes for attaching tin-lead or lead-free eutectic spheres. Red dye supports pre-flow visual inspection. WS600 Red provides standard viscosity, WS600MHV Red adds higher viscosity for stencil printing, high-humidity conditions, and hot-slump control, and WS600L Red provides lower viscosity. The series is halide-free and uses a completely water-soluble carrier resin. Typical family data include approximately eight hours of stencil life at 40-60% RH and 20-25 deg C, greater than 100,000 ohm-cm water-extract resistivity, and a typical residue pH of 6.8. Sealed storage is specified at 15-25 deg C without refrigeration.

Key features

  • Variant-controlled rheology: Standard, higher-, and lower-viscosity grades address distinct assembly conditions.
  • Pre-flow inspection aid: Red dye improves visibility before sphere-attach processing.
  • Water-soluble halide-free system: The carrier resin is completely water-soluble and contains no halide.

Applications

BGA and CSP sphere attach, stencil printing, repair, and rework using the selected WS600 variant.

Product Family

ALPHA WS600

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical series data; viscosity values remain tied to the named variant.

PropertyValueUnitMethod / condition
ColorDeep amber or deep redVisual
Stencil lifeApprox. 8hours40-60% RH, 20-25 deg C
Water-extract resistivity> 100,000ohm-cmTypical
Halide contentHalide-freeChemical property
Flux-residue pH6.8Typical
WS600 viscosityApprox. 600PoiseSpiral/Malcom, 5 rpm
WS600MHV viscosityApprox. 800PoiseSpiral/Malcom, 5 rpm
WS600L viscosityApprox. 500PoiseSpiral/Malcom, 5 rpm