ALPHA WS362

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA WS362

Main features

  • High-activity, 25% solids water-soluble flux designed for densely packed assemblies and multilayer boards requiring relatively high preheat temperatures.
  • Highly water-soluble post-solder residues support effective cleaning for high ionic cleanliness and surface insulation resistance.
  • Halide-free formulation with rapid wetting and support for foam, spray, or wave application techniques.

Product Description

ALPHA WS362-25 Water-Soluble Surface Mount Flux is a halide-free, water-soluble organic flux designed for soldering surface mount and mixed technology assemblies where effective residue removal and high ionic cleanliness are important. Its high-activity, 25% solids formulation is recommended for densely packed assemblies and multilayer boards requiring relatively high preheat temperatures. After soldering, the highly water-soluble residues can be readily removed, supporting high ionic cleanliness and surface insulation resistance. ALPHA WS362-25 can be applied by foam, spray, or wave techniques and is designated ORMO according to IPC J-STD-004.

Key features

  • Highly water-soluble residue: Designed for effective post-solder cleaning where high ionic cleanliness is required.
  • High activity and 25% solids: Recommended for densely packed assemblies and multilayer boards requiring relatively high preheat temperatures.
  • Halide-free formulation: Provides rapid wetting and carries an ORMO designation according to IPC J-STD-004.
  • Multiple application methods: Suitable for foam, spray, and wave application techniques.

Applications / Suitable for

  • Surface mount assemblies
  • Mixed technology assemblies
  • Densely packed assemblies requiring effective residue cleaning
  • Multilayer boards requiring relatively high preheat temperatures
Product Family

ALPHA WS362

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids Solids
25 %
Specific Gravity Specific Gravity
0.846 ± 0.005 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Selected typical properties of ALPHA WS362-25 in its as-supplied liquid state.

Property Value Unit Method or condition
Appearance Clear, pale yellow - As supplied
Solids content 25 wt/wt % Typical value
Specific gravity 0.846 +/- 0.005 - 25 °C (77 °F)
Acid number 33.00 +/- 2.00 mg KOH/g Typical value
pH 3.2 - 5% aqueous solution
Flash point 17 °C T.C.C.
Technical properties

After-processing / final-state properties

Surface insulation resistance results for ALPHA WS362-25 after hydrocleaning under the stated IPC J-STD-004 test conditions.

Property Result Requirement Method or condition
Surface insulation resistance - Comb-Down, hydrocleaned 4.4 x 108 ohms >1.0 x 108 ohms IPC J-STD-004; 85 °C/85% RH, 7 days; -50 V, measurement at 100 V on IPC B-24 board
Surface insulation resistance - Control Boards 3.6 x 109 ohms >1.0 x 109 ohms IPC J-STD-004; 85 °C/85% RH, 7 days; -50 V, measurement at 100 V on IPC B-24 board

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers