ALPHA TRUEHEIGHT

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA TRUEHEIGHT

Main features

  • Non-collapse copper spacer provides precise, repeatable component standoff height with thickness tolerances as low as +/- 0.010 mm.
  • Nickel/gold finish covers all sides of the copper disc to maintain a solderable surface without exposed copper after reflow.
  • Tape-and-reel packaging enables automated placement with standard pick-and-place equipment for integration into SMT assembly processes.

Product Description

ALPHA TrueHeight Spacer is a non-collapse copper disc with nickel and gold surface finishes designed to provide a precise, repeatable standoff height for electronic components during reflow soldering. The solderable spacer can be automatically placed using standard pick-and-place equipment onto PCB pads printed with solder paste, supporting integration into standard SMT assembly processes. Available dimensional tolerances are as low as +/- 0.010 mm depending on spacer size. Its fixed-height function can support applications where component warpage, tilt, solder bond-line control, or component-to-PCB clearance are important.

Key features

  • Precise standoff control: Non-collapse construction provides a fixed and repeatable component standoff height, with available thickness tolerances as low as +/- 0.010 mm.
  • Solderable nickel/gold finish: Copper discs are coated with a nickel barrier layer and gold finish, with all sides coated so copper is not exposed after reflow.
  • Automated assembly integration: Tape-and-reel packaging supports fast placement using standard pick-and-place equipment and integration into standard assembly processes.

Applications / Suitable for

  • Maintaining minimum standoff height for BGA packages affected by excessive warping during reflow
  • Preventing component tilt and providing a fixed solder bond line under large-area LGAs and power packs
  • Providing component-to-PCB clearance for reflow soldering of through-hole components
Product Family

ALPHA TRUEHEIGHT

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Selected construction, dimensional, and packaging properties of ALPHA TrueHeight Spacers.

Property Value Unit Method / condition
Construction Copper with nickel/gold finish - All ALPHA TrueHeight Spacer sizes
Disc diameter 0.50 or 0.76 mm Dimension 'a'; tolerance +/- 0.05 mm
Available thickness 0.10, 0.25, 0.30, 0.34, 0.38 mm Dimension 'b'; availability depends on disc diameter
Thickness tolerance +/- 0.010 to +/- 0.020 mm Depends on nominal thickness: 0.10 +/- 0.010; 0.25 +/- 0.013; 0.30 +/- 0.015; 0.34 +/- 0.017; 0.38 +/- 0.020 mm
Carrier tape width 8 mm Tape dimension W; all sizes
Tape pitch P0 / P1 4 / 2 mm Tape dimensions; all sizes