ALPHA SM351F

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA SM351F

Main features

  • Fast-Wetting Foam and Wave Flux
  • Tack-Free Pin-Testable Residue
  • Halide-Free Low-Solids Formulation

Product Description

ALPHA SM-351F Liquid Soldering Flux uses a low-solids no-clean liquid formulation without halides, rosin, or resin for foam and wave soldering. It is designed for fast wetting and leaves a very small amount of barely visible, tack-free, noncorrosive residue. This residue profile supports accurate pin testing and eliminates a required post-solder cleaning step under the documented use conditions. The flux is classified ORL0 under IPC J-STD-004 and L3NC under IPC-SF-818. As supplied, it contains 2.1% solids, has an 11 deg C flash point, and carries a 540-day shelf life. Typical specific gravity is 0.812 +/- 0.005 at 25 deg C; acid number is 16.5 +/- 1.0 mg KOH/g.

Key features

  • Halide- and rosin-free: Low-solids formulation supports no-clean electronics soldering.
  • Fast wetting: Designed for efficient foam and wave soldering application.
  • Tack-free noncorrosive residue: Barely visible residue supports accurate pin testing without required cleaning.

Applications

Foam or wave soldering for electronic circuit assemblies.

Product Family

ALPHA SM351F

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids Solids
2.1 %
Specific Gravity Specific Gravity
0.812 ± 0.005 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear, pale-yellow liquidTypical
Solids content2.1% by weightTypical
Specific gravity0.812 +/- 0.00525 deg C
Acid number16.5 +/- 1.0mg KOH/gTypical
Flash point11deg CT.C.C.
Shelf life540daysFrom date of manufacture
Flux classificationORL0IPC J-STD-004