ALPHA SC-7525 Cleaner

Harmonization Code : 3810.90.90 | Fluxes and other auxiliary preparations for soldering, brazing, welding

ALPHA SC-7525 Cleaner

Main features

  • IPA alternative
  • High solvency
  • Suitable for manual & immersive methods

Product Description

ALPHA SC-7525 Cleaner is a chemically active solvent developed to effectively replace isopropyl alcohol (IPA) in various manual and equipment cleaning applications.

SC-7525 is a blend of alcohols, aliphatic hydrocarbons, and orange terpenes. The combination of polar and non-polar components makes it especially suitable for removing all types of solder paste residues from stencils and misprinted printed circuit boards (PCBs).

Product Key Features

  • High-performance alternative to Isopropyl Alcohol (IPA)
  • Highly effective at dissolving and removing all types of solder paste from stencils and misprinted assemblies.

Applications

  • Suitable for use in various manual and equipment-related cleaning processes.
Product Family

ALPHA SC-7525

1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Colorless to slight yellow
Specific Gravity Specific Gravity
0.7868
Thermal Properties
Flash Point Flash Point
15.6 °C