ALPHA RMA390

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

ALPHA RMA390

Main features

  • Wide reflow profile window supporting air and nitrogen reflow with straight-ramp or soak profiles up to 300 °C.
  • ROL0, halide-free rosin-based paste flux whose post-reflow residue is suitable to remain on the circuit board without cleaning.
  • Flexible application by screen printing, pin transfer, doctor blade, dip coating, or dispensing, with documented SIR and electromigration performance.

Product Description

ALPHA RMA-390-DH6 Paste Flux is a rosin-based paste flux designed for surface mount and other demanding electronic assembly applications. Its activator system is formulated to penetrate moderately tarnished surfaces, while the post-reflow residue is suitable to remain on the circuit board without cleaning. The flux supports air and nitrogen reflow using straight-ramp or soak profiles up to 300 °C and provides documented electrical reliability performance. ALPHA RMA-390-DH6 is classified ROL0 according to IPC J-STD-004 and can be applied by screen printing, pin transfer, doctor blade, dip coating, or dispensing.

Key features

  • Wide reflow profile window: Supports straight-ramp or soak profiles in both air and nitrogen reflow up to 300 °C.
  • No-clean residue capability: Post-reflow residue is suitable to remain on the circuit board without cleaning.
  • ROL0, halide-free formulation: Classified ROL0 per IPC J-STD-004, with halide-free status based on formulation.
  • Flexible application methods: Supports screen printing, pin transfer, doctor blade, dip coating, and dispensing.

Applications / Suitable for

  • Surface mount electronic assembly
  • High-density PWB assemblies
  • Applications involving moderately tarnished soldering surfaces
  • Screen printing, pin transfer, doctor blade, dip coating, and dispensing processes
Product Family

ALPHA RMA390

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Selected physical and chemical properties of ALPHA RMA-390-DH6 Paste Flux in its as-supplied state.

Property Value Unit Method / condition
Appearance Smooth, amber paste - As supplied
Viscosity 110 to 400 Poise Typical; Malcom Viscometer, 5 rpm at 25 °C
Fineness of grind <10 µm Physical property
Activity level ROL0 - IPC J-STD-004
Halide content Halide-free - Based on formulation
Technical properties

After-processing / final-state properties

Selected corrosion and electrical test results for ALPHA RMA-390-DH6 under the stated test conditions.

Property Result Method / condition
Copper mirror corrosion Pass IPC J-STD-004
SIR Pass, 2.5 x 1011 ohms Bellcore GR78-CORE; 96 hours at 35 °C/85% RH; pass ≥1 x 1011 ohms
Electromigration Pass, 2.2 x 1010 ohms Bellcore GR78-CORE; 500 hours at 65 °C/85% RH, 10 V; pass = final > initial/10
IPC SIR Pass, 1.1 x 109 ohms IPC J-STD-004A; 7 days at 85 °C/85% RH; pass >108 ohms
HP electrochemical migration Pass HP ECM; 28 days at 50 °C/90% RH, 10 V