ALPHA HF-1

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA HF-1

Main features

  • Wide reflow profile window supporting air and nitrogen reflow with straight-ramp or soak profiles up to 300 °C.
  • ROL0, halide-free flux system with residue suitable to remain on the circuit board without cleaning.
  • Broad rework capability covering touch-up, hand soldering, BGA repair/re-balling, and QFN/LGA repair.

Product Description

ALPHA HF-1 Flux Gel is a rosin-based paste flux for surface-mount rework and other demanding electronic assembly operations. Its activator system can penetrate moderately tarnished surfaces, while the post-reflow residue can remain on the circuit board without cleaning. The flux supports both air and nitrogen reflow with straight-ramp or soak profiles up to 300 °C and is classified ROL0 according to IPC J-STD-004. Its paste form supports several application methods, including dispensing, screen printing, pin transfer, doctor blade, and dip coating. Documented rework uses include touch-up and hand soldering, BGA repair and re-balling, and QFN/LGA repair.

Key features

  • Wide reflow profile window: Supports air and nitrogen reflow using straight-ramp or soak profiles up to 300 °C.
  • ROL0, halide-free flux system: Classified ROL0 per IPC J-STD-004 and identified as halide-free based on formulation.
  • Broad rework capability: Supports touch-up and hand soldering as well as BGA repair/re-balling and QFN/LGA repair.

Applications / Suitable for

  • Surface-mount rework
  • Touch-up and hand soldering
  • BGA repair and re-balling
  • QFN/LGA repair
Product Family

ALPHA HF-1

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Selected physical and chemical properties of ALPHA HF-1 Flux Gel in its as-supplied paste state.

Property Value Unit Method / condition
Appearance Smooth, amber paste - As supplied
Viscosity 400 to 1000 Poise Malcom Viscometer, 5 rpm at 25 °C
Fineness of grind <10 µm Physical property
Activity level ROL0 - IPC J-STD-004
Halide content Halide-free - Based on formulation
Technical properties

After-processing / final-state properties

Selected electrical test results for ALPHA HF-1 Flux Gel under the stated environmental test conditions.

Property Value Unit Method / condition
SIR Pass, 2.5 x 1011 ohms Bellcore GR78-CORE; 96 hours at 35 °C/85% RH; pass ≥1 x 1011 ohm
Electromigration Pass, 2.2 x 1010 ohms Bellcore GR78-CORE; 500 hours at 65 °C/85% RH, 10 V; pass = final > initial/10
IPC SIR Pass, 1.1 x 109 ohms IPC J-STD-004A; 7 days at 85 °C/85% RH; pass >108 ohms
HP electrochemical migration Pass - HP ECM; 28 days at 50 °C/90% RH, 10 V