ALPHA EF6100

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA EF6100

Main features

  • Alloy-Specific Wave Process Control
  • Low-Solids Pin-Testable Residue
  • High-Reliability No-Clean Soldering

Product Description

ALPHA EF-6100 Liquid Soldering Flux is a low-solids, no-clean, alcohol-based flux for lead-free and tin-lead wave and selective soldering. It is applied by spray and is designed for through-hole fill with reduced solder balling, bridging, and skips while leaving low residues compatible with pin testing. Typical solids content is 3.8%, and the acid number is controlled to 22.8 to 25.2 to maintain solids during use. Process guidance separates SAC305/SACX0307 and Sn63Pb37 settings, including alloy-specific flux loading, preheat, contact time, and solder-pot temperature. Residues are designed to remain on the board but can be removed with aqueous or solvent cleaners when needed.

Key features

  • Alloy-specific spray process: Separate SAC305/SACX0307 and Sn63Pb37 settings define flux loading, preheat, contact time, and solder-pot conditions.
  • Low-solids no-clean residue: A 3.8% solids formulation leaves low residue for no-clean assembly and supports pin-test access.
  • SIR and electromigration performance: Uncleaned residues pass the listed IPC, Bellcore, and JIS surface-insulation-resistance and electromigration tests under specified conditions.

Applications

Used for lead-free and tin-lead wave or selective soldering where spray fluxing, controlled alloy-specific process settings, and low no-clean residue are required.

Product Family

ALPHA EF6100

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids Solids
3.8 %
Specific Gravity Specific Gravity
0.794 ± 0.003 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear, colorless to pale yellow liquidTypical
Solids content3.8% by weightTypical
Specific gravity0.794 +/- 0.003At 25 deg C (77 deg F)
Acid number23.9 +/- 1.2mg KOH/gTypical
pH3.35% aqueous solution
Flash point12 (53)deg C (deg F)T.C.C.
Shelf life360daysFrom date of manufacture
IPC classificationORL0IPC J-STD-004