ALPHA 611 RMA Flux is an amber, mildly activated rosin liquid flux formulated for foam application in electronics soldering. Its 37% solids content provides full flux coverage on dense plated-through-hole circuit boards, while the water-white gum rosin and non-ionic activator system support consistent RMA processing. Typical specific gravity is 0.896 +/- 0.005 at 25 deg C. Flux residues are non-conductive and non-hygroscopic and are considered non-corrosive in most applications. Critical assemblies can be cleaned with a compatible solvent cleaner or an aqueous cleaner such as ALPHA 2110.

Key features

  • Dense-board foam coverage: The 37% solids formulation provides effective flux coverage on dense plated-through-hole circuit boards.
  • Mildly activated rosin system: Water-white gum rosin and non-ionic activators support controlled RMA soldering performance.
  • Removable RMA residues: Critical assemblies can be cleaned with a compatible solvent or an aqueous cleaner such as ALPHA 2110.

Applications

Applications include foam fluxing for wave soldering of dense plated-through-hole circuit boards and other supported RMA soldering processes.

Product Family

ALPHA 611

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids Solids
37 %
Specific Gravity Specific Gravity
0.896 ± 0.005 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Technical values are typical for ALPHA 611 as supplied.

PropertyValueUnitMethod / condition
AppearanceAmber liquidAs supplied
Solids content37%Typical
Specific gravity0.896 +/- 0.00525 deg C
Weight per gallon7.45lb/gal25 deg C
Flash point17deg CT.C.C.
Water-extract resistivity250,000ohm cmTypical
Shelf life720daysFrom date of manufacture