AEROWAX HT

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

AEROWAX HT

Main features

  • 82 to 88 deg C Melting Range
  • Chemical-Resistant Selective-Plating Maskant
  • UV-Detectable BIOACT-Removable Coating

Product Description

AEROWAX™ HT Wax Maskant is a highly refined platers wax for selective plating operations. Supplied in slab form, it has a melting-point range of 82–88°C (180–190°F) and is used to mask both simple and complex part geometries during hard chrome, nickel sulfamate, and other selective plating processes. The wax combines adhesion and flexibility with resistance to crazing, cracking, elevated process temperatures, and harsh plating chemicals. It is detectable under UV light for inspection and can be removed using Petroferm BIOACT® 280 series dewaxing agents. One-tank and two-tank dip processes are documented, with a minimum of two wax coats recommended.

Key features

  • Selective-plating maskant for simple and complex geometries.
  • High-temperature wax with an 82–88°C (180–190°F) melting-point range.
  • Adhesive and flexible coating that resists crazing and cracking.
  • Resistant to harsh plating chemicals under the intended process conditions.
  • UV detectable to support inspection of the applied wax mask.
  • Removable with Petroferm BIOACT® 280 series dewaxing agents.

Applications / Suitable for

  • Hard chrome selective plating.
  • Nickel sulfamate selective plating.
  • Other selective plating operations requiring a removable wax maskant.
Product Family

AEROWAX HT

Loading pricing…

Technical Specifications

No specifications available.

Additional Information

High-temperature wax maskant

AEROWAX™ HT Wax Maskant

A highly refined platers wax for masking simple and complex part geometries during hard chrome, nickel sulfamate, and other selective plating operations. The wax combines adhesion and flexibility with high-temperature stability, chemical resistance, UV detectability, and removal using compatible BIOACT® dewaxing agents.

82–88°C melting range Slab form UV detectable Chemical resistant 36-month shelf life

As supplied

As-supplied properties

Typical property data are provided for product evaluation and are not specification limits.

Property Typical value Context
Form Slabs As supplied
Melting-point range 82–88°C (180–190°F) Typical
Needle penetration Approximately 18 dmm At 25°C
Kinematic viscosity 16.5–21 mm²/s At 100°C
Processing

Masking process

Add AEROWAX™ HT to the tank reservoir and apply heat. Use clean, dry parts and apply a minimum of two wax coats. Build the coating through repeated dipping until the required mask thickness is reached.

Two-tank process — first coat: Heat the first tank to 118°C ± 9°C (245°F ± 15°F). Immerse the clean, dry part until it reaches the wax-bath temperature, then remove and cool slightly.
Two-tank process — subsequent coats: Heat the second tank to approximately 93°C (200°F). Dip and withdraw the part quickly, allow it to cool slightly, and repeat until the desired thickness is achieved.
One-tank process: Heat the tank to 110°C ± 5°C (230°F ± 10°F). Immerse the clean, dry part until it reaches bath temperature, remove and cool slightly, then repeat quick dip-and-withdraw cycles for subsequent coats.
Coating build: Apply at least two coats and continue until the wax mask reaches the thickness required for the specific part geometry and plating process.

 

Post-process

Wax removal

After plating, remove AEROWAX™ HT using Petroferm BIOACT® 280 series dewaxing agents. Establish the removal process for the part geometry, wax thickness, and applicable cleaning conditions, and follow the current cleaning-agent instructions and safety documentation.

Storage and packaging

AEROWAX™ HT is available in 60 lb (27 kg) cartons. Shelf life is 36 months when stored in the original sealed container above 10°C (50°F). Consult the current Safety Data Sheet for handling and disposal requirements.

Use contexts

Applications

AEROWAX™ HT is used as a removable mask during selective plating. Final process suitability depends on part cleanliness, geometry, wax thickness, bath conditions, plating chemistry, and dewaxing requirements.

Hard chrome plating
Masks selected surfaces of simple or complex parts during hard chrome plating operations.
Nickel sulfamate plating
Provides a removable wax barrier for selective nickel sulfamate plating processes.
Complex selective masking
Supports repeated dip coating of complex geometries where adhesion, flexibility, chemical resistance, and UV inspection are useful process characteristics.
Next steps

Evaluate AEROWAX™ HT for your selective plating process

Contact Krayden to discuss part geometry, tank configuration, wax temperature, coating build, plating chemistry, UV inspection, removal using BIOACT® dewaxing agents, packaging availability, and process trials.