Aculon HB | Hydrophilic Treatment

Harmonization Code : 34021900 | Surface active agents

Aculon HB | Hydrophilic based

Main features

  • Used as provided for wipe applications
  • Use for dip treatment applications
  • Gentle enough for many substrates.

Product Description

Aculon's HB  is a water-based specialty coating capable of supplying hydrophilic properties across a broad spectrum of metal or glass surfaces. It is quick and easy to apply and in some cases may also be used on plastics.

Aculon HB: Aculon HB is a water-based coating product that imparts hydrophilic functionality to multiple substrate types. 

Technical Specifications

General Properties
Specific Gravity Specific Gravity
1.1

Additional Information

 

How to apply the Aculon HB

STEP 1 ⇨ CLEAN

STEP 2 ⇨ TREAT

STEP 3 ⇨ DRY

 

Parts must be sufficiently clean before treatment for proper bonding and effective application.

To clean, solvents or soap and water can be used to degrease the substrate.

Then, a cleaner is recommended to remove monolayer-scale contaminants.

 

 

Wipe - With the wipe, thoroughly apply pressure to the location where the hydrophilic properties are required

This product does not require a cure, however, in some cases and substrates a brief 5-minute cure at 60⁰C will benefit. 

Dip - Fully immerse the part in the treatment solution for 1 minute, then remove the substrate.

 

Application Tips

  • If any bath will be subject to environmental contamination, recirculate the solution through a 0.2-micron polypropylene media filter.
  • Dip tanks should be made of polypropylene or PTFE polymers.
  • The product should be used at room temperature.
  • Coat the substrate as soon as possible after cleaning to prevent recontamination.
  • This material may be reapplied as needed.
  • Dry temperatures and conditions should be optimized based on substrate and durability requirements.

 

 

Leading Brands Trust in Our Products and Services