ABLESTIK G757HF-D

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

ABLESTIK G757HF-D

Main features

  • Automotive Headlamp Lens Bonding
  • Thixotropic Sag-Resistant Placement
  • Flexible -40 to 150 deg C Operation

Product Description

LOCTITE ABLESTIK G757HF-D is a one-part, gray, thixotropic epoxy adhesive for bonding automotive headlamp lenses to reflectors. The heat-cure material is supported on glass, steel, copper, aluminum, and fiber-reinforced plastic. Its 400 mil sag-resistance value and thixotropic behavior keep the applied adhesive in place during assembly. Recommended cure options are 45 minutes at 140 deg C, 20 minutes at 160 deg C, or 10 minutes at 180 deg C. The cured adhesive remains flexible across its stated -40 to 140 deg C operating range and has a typical aluminum-to-aluminum lap shear strength of 10 N/mm^2 at 25 deg C.

Key features

  • Headlamp lens-to-reflector bonding: The one-part adhesive is specifically intended for automotive headlamp lens and reflector assembly.
  • Flexible temperature performance: The cured adhesive remains flexible across the stated -40 to 140 deg C operating range.


Applications

Applications include bonding automotive headlamp lenses to reflectors using supported glass, metal, and fiber-reinforced plastic surfaces.

Product Family

ABLESTIK G757HF-D

Loading pricing…

Technical Specifications

General Properties
Appearance Appearance
Gray
Density (g) Density (g)
1.15 g/cm3
Pot Life Pot Life
1 months
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
130.2 °C
Operating Temperature Operating Temperature
-40 to +140 °C
Physical Properties
Viscosity Viscosity
275,000 mPa.s
Electrical Properties
Surface Resistivity Surface Resistivity
1.1×10¹⁸ Ohms/sq
Volume Resistivity Volume Resistivity
1.2×10¹⁸ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Technical values are typical; cure schedules are guideline recommendations.

Property Value Unit Method / condition
Appearance Gray   As supplied
Density 1.15 g/cm^3 Typical
Sag resistance 1.8 mm 25 deg C
Press flow 100 seconds Typical
Storage life 6 months 0 deg C
Cure schedule 45 at 140; 20 at 160; 10 at 180 minutes at deg C Guideline heat-cure options
Technical properties

After-processing / final-state properties

Final-state values are typical for cured LOCTITE ABLESTIK G 757 under the stated test conditions.

Property Value Unit Method / condition
Operating temperature -40 to 140 deg C Product operating range
Shore D hardness 42   25 deg C
Shore A hardness 85   120 deg C
Tensile peel strength 1.75 N/mm^2 Aluminum-to-aluminum; 25 deg C
Tensile lap shear strength 10 N/mm^2 Aluminum-to-aluminum; 25 deg C