Loctite Ablestik 84-3LV

Main features

  • Solvent-free
  • Long work life
  • One component

Product Description

LOCTITE ABLESTIK 84-3LV adhesive is designed for die attach applications. It is a non conductive, solvent free material that is used as an electrically insulating adhesive.

LOCTITE ABLESTIK 84-3LV is a Low Viscosity version of LOCTITE ABLESTIK 84-3. It can be applied by stamping or syringe dispensing.

 

Cure Schedule

  • 1 hour @ 150°C 
  • 2 hours @ 125°C

Technical Specifications

General Properties
Work life @25°C Work life @25°C
336 hours
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
66 °C
Thermal Conductivity Thermal Conductivity
0.5 W/m.K
Weight Loss @ 300°C Weight Loss @ 300°C
0.12 %
Physical Properties
Thixotropic index Thixotropic index
1.6
Viscosity Viscosity
12,500 mPa.s