LOCTITE ABLESTIK 84-3J

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK 84-3J

Main features

  • Bondline control
  • Box oven Cure
  • Non Conductive

Product Description

LOCTITE ABLESTIK 84-3J electrically insulating epoxy adhesive is designed for die attach applications as well as component attach. The use of this material as a staking compound under chip components help eliminate shorting due to the capillary action of conductive adhesives.

LOCTITE ABLESTIK 84-3J non conductive adhesive has a long work life and is engineered with spacers for accurate bondline control. It has a lower viscosity and a similar resin system and outgassing to 84-3 (that comes with MIL certification) and can be used for sensor die attach.

Cure Schedule

  • 1 hour @ 150°C
  • 2 hours @ 125°C
Product Family

ABLESTIK 84-3J

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 55 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C Work life @25°C
336 hours
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
87 °C
Thermal Conductivity Thermal Conductivity
0.5 W/m.K
Weight Loss @ 300°C Weight Loss @ 300°C
0.17 %
Physical Properties
Thixotropic index Thixotropic index
2.5
Viscosity Viscosity
20,000 mPa.s