LOCTITE ABLESTIK 8008HT

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik 8008HT

Main features

  • Thermally conductive
  • Low modulus
  • Stencil printing

Product Description

LOCTITE® ABLESTIK 8008HT adhesive is designed for high power devices in high UPH environment. It offers a lead-free alternative to soft solder and eutectic and can potentially reduce the layers of backside metallization required. This material can be applied to a wafer backside by stencil printing and then B-staged in an oven. The adhesive can then be cured after die attach in an in-line process exhibiting a consistent, void-free bondline without bleed.

LOCTITE ABLESTIK 8008HT should be used with a pressure sensitive dicing tape and is not compatible with UV dicing tapes. This hybrid chemistry product is thermally and electrically conductive and can be snap cured after B-stage.

 

Cure Schedule

  • 20 seconds @ 170°C. (Snap Cure)
  • 30 minutes ramp to 175°C + 60 minutes @ 175°C (Air box oven Cure)

Technical Specifications

General Properties
Work life @25°C Work life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
264 °C
Thermal Conductivity Thermal Conductivity
11 W/m.K
Chemical Properties
Moisture absorption Moisture absorption
0.53 %
Physical Properties
Thixotropic index Thixotropic index
4.0
Viscosity Viscosity
50,000 mPa.s