LOCTITE ABLESTIK 8008

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik 8008HT

Main features

  • Snap curable after B stage
  • Low modulus
  • Void free bondline without bleed

Product Description

LOCTITE® ABLESTIK 8008 snap curable adhesive is designed for small die sizes (an be applied to a wafer backside by stencil printing and then B-staged in an oven. The adhesive can then be cured after die attach in an in-line process exhibiting a consistent, void-free bondline without bleed.

LOCTITE ABLESTIK 8008 should be used with a pressure sensitive dicing tape and is not compatible with UV dicing tapes.

Product Family

ABLESTIK 8008

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C Work life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
270 °C
Thermal Conductivity Thermal Conductivity
2.2 W/m.K
Physical Properties
Thixotropic index Thixotropic index
2.6
Viscosity Viscosity
48,000 mPa.s