3M EZ250150

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M EZ250150

Main features

  • Extended 2 to 4 Minute Open Time
  • Aluminum or Glass to Wood or Plastic
  • Flexible Cured Adhesive Layer

Product Description

3M Scotch-Weld PUR Easy 250 Plastic Adhesive EZ250150 is a one-component, 100% solids moisture-curing polyurethane reactive adhesive for longer assembly windows on larger or more complex parts. Applied warm at 121 deg C, it provides an open time of 2 to 4 minutes and a set time of 30 to 150 seconds. Supported combinations include wood-to-wood, plastic-to-plastic, wood-to-plastic, aluminum-to-wood or plastic, and glass-to-wood or plastic. A typical elongation at break of 700% after seven days at 23 deg C indicates a flexible cured adhesive layer that can deform before breaking. Moisture access is required, so metal-to-metal, glass-to-glass, and metal-to-glass bonds are excluded.

Key features

  • Longer assembly window: An open time of 2 to 4 minutes and a set time of 30 to 150 seconds support larger or more complex assemblies.
  • Supported substrate combinations: Bonds wood and plastics and joins aluminum or glass to wood or plastic while preserving moisture-access limits.
  • Flexible cured adhesive layer: A typical 700% elongation at break indicates a cured layer that can deform before breaking rather than acting as a rigid bondline.

Applications

Applications include larger or more complex wood, plastic, aluminum-to-wood or plastic, and glass-to-wood or plastic assemblies that benefit from the longer open and set window.

Technical Specifications

General Properties
Color Color
White / Off - White
Physical Properties
Viscosity Viscosity
9,000 mPa.s
Mechanical Properties
Elongation Elongation
700 %

Additional Information

Technical properties

As-supplied / before-processing properties

Open and handling times are approximate and depend on adhesive temperature and application conditions.

PropertyValueUnitMethod / condition
Color, solidWhite to off-whiteAs supplied
Viscosity9,000cP121 deg C; Brookfield Thermosel, spindle No. 27
Density, molten9.1lb/galTypical
Solids content100%Typical
Application temperature121deg C250 deg F
Open time2 to 4minutesProduct feature range
Set time30 to 150secondsProduct feature range

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers