3M EZ250120

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M EZ250120

Main features

  • Medium-Set Wood Assembly
  • Thin-Bondline Warm Application
  • Moisture-Curing One-Part Processing

Product Description

3M Scotch-Weld PUR Easy 250 Wood Adhesive EZ250120 is a one-component, 100% solids moisture-curing polyurethane reactive adhesive for wood, wood-based surfaces, and selected plastics. Applied warm at 121 deg C, its low-viscosity melt is designed for thin glue lines. The supported open-time range is 1.5 to 4 minutes, and the set-time range is 15 to 120 seconds, providing a medium-set process for wood assembly. Cure rate depends on air temperature, relative humidity, substrate type, and bondline thickness. Moisture must reach the bondline; the adhesive is not suitable for metal-to-metal, glass-to-glass, or metal-to-glass bonding because those substrate pairs do not provide enough moisture for cure.

Key features

  • Medium-set assembly window: An open time of 1.5 to 4 minutes and a set time of 15 to 120 seconds support efficient wood assembly.
  • Thin glue-line processing: A typical viscosity of 3,000 cP at 121 deg C supports controlled application in thin bondlines.
  • Moisture-dependent cure: Cures with available moisture, defining suitable substrate pairs and excluding metal-to-metal, glass-to-glass, and metal-to-glass bonds.

Applications

Applications include wood and wood-based assembly, thin glue-line bonding, and selected plastic bonding where the joint and process provide moisture for cure.

Technical Specifications

General Properties
Color Color
White/ Off - White
Physical Properties
Viscosity Viscosity
3000 mPa.s
Mechanical Properties
Elongation Elongation
625 %

Additional Information

Technical properties

As-supplied / before-processing properties

Open and handling times are approximate and depend on adhesive temperature and application conditions.

PropertyValueUnitMethod / condition
Color, solidWhite to off-whiteAs supplied
Viscosity3,000cP121 deg C; Brookfield Thermosel, spindle No. 27
Density, molten8.9lb/galTypical
Solids content100%Typical
Application temperature121deg C250 deg F
Open time1.5 to 4minutesProduct feature range
Set time15 to 120secondsProduct feature range

Leading Brands Trust in Our Products and Services