Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Structural Polyurethane Adhesive DP609

Main features

  • Rapid room-temperature curing
  • Flexible structural bonding
  • Approx. 9-minute work life at 23°C

Product Description

3M Scotch-Weld EPX Adhesive DP609 is designed for fast curing at room temperature and delivers strong, durable bonds across a variety of materials. It is particularly effective for bonding plastics as well as painted or primed metal surfaces. With excellent flow from the cartridge and non-sag properties, the adhesive is easy to apply—even on vertical surfaces—while offering reliable gap-filling capability. The product develops handling strength within approximately one hour and continues to build full strength over time, ensuring long-term performance and durability even in demanding conditions and low-temperature environments.

Product Key Features

  • Rapid room-temperature curing for efficient application and assembly
  • Flexible structural bonding suitable for plastics and coated metals
  • Approx. 9-minute work life at 23°C for precise positioning before bonding
  • Handling strength in ~1 hour for faster processing
  • Full strength builds over 24 hours, with continued improvement over time
  • Excellent flow and non-sag formulation for clean application on vertical surfaces
  • Strong gap-filling capability for uneven or irregular joints
  • High flexibility and strain tolerance for durable, long-lasting bonds
  • Maintains performance across a wide temperature range, including low temperatures
  • High toughness and strength retention in demanding environments
Product Family

3M DP609

1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Please select Package Type and Color.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Polyol/Isocyanate
Color Color
Off-White/Brown
Mix Ratio Mix Ratio
1:1
Specific Gravity Specific Gravity
1.03 - 1.12
Work life @25°C Work life @25°C
0.15 hours
Physical Properties
Viscosity Viscosity
10,000 - 55,000 mPa.s

Leading Brands Trust in Our Products and Services