3M™ Scotch-Weld™ DP460

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M™ Scotch-Weld™ 460

Main features

  • High shear strength
  • 60-minute work life
  • Easy mixing

Product Description

3M™ Scotch-Weld™ Epoxy Adhesives DP460 is a high performance, two-part epoxy adhesive offering outstanding shear and peel adhesion, and very high levels of durability.

Product Key Features

  • High shear strength
  • 60 minute work life
  • Easy mixing
  • High peel strength

Applications

  • Structural bonding of metals, composites, and plastics
  • Automotive and transportation assemblies
  • Aerospace interior and non-critical structural components
  • Bonding panels, brackets, and enclosures
  • Industrial equipment fabrication and repair
  • Electronics housing and component assembly
  • General-purpose maintenance and manufacturing bonding
Product Family

3M DP460

1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Please select Package Type and Color.
TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity Viscosity
20,000-50,000 mPa.s
General Properties
Color Color
white/amber
Mix Ratio Mix Ratio
2:1
Work life @25°C Work life @25°C
60 minutes hours
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.18 W/m.K
Electrical Properties
Volume Resistivity Volume Resistivity
2.4e+14 Ohms⋅cm