3M™ Scotch-Weld™ Epoxy Adhesive DP110

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Epoxy Adhesive DP110

Main features

  • Controlled flow
  • 20-minute handling strength
  • Good adhesion to many plastics and metals

Product Description

3M™Scotch-Weld™ Epoxy Adhesive DP110 is a flexible, fast-curing, two-part structural epoxy. It provides excellent shear and peel strength while remaining highly adaptable to thermal expansion and vibration.

Product Key Features

  • Controlled flow
  • 20 minute handling strength
  • Duo-Pak cartridge dispensing system
  • Good adhesion to many plastics and metals

Applications

  • Signage & Display Assembly: Bonding plastic lettering or transparent panels to metal frames with invisible seams.
  • Sporting Goods Manufacturing: Assembling composite, metal, or fiberglass parts that require high impact resistance.
  • General Industrial Bonding: Joining dissimilar substrates (like aluminum to plastic) prone to thermal movement.
  • Electronic Component Encapsulation: Securing parts and sealing joints against moisture without high visual opacity.
Product Family

3M DP110

1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Please select Package Type and Color.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Modified Epoxy
Color Color
Yellow Translucent
Mix Ratio Mix Ratio
1:1