3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus

Main features

  • 2-5 minute work life
  • Good shear and excellent peel strength
  • Flexible

Product Description

3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus is a flexible, fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is unique among fast setting mercaptan cure epoxies in that it combines high shear strength with good peel performance properties. Scotch-Weld epoxy adhesive DP100 Plus Clear is clear when cured. Available in bulk containers as 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus B/A Clear.

Product Key Features

  • 2-5 minute worklife
  • Good shear and excellent peel strength
  • Flexible
  • 1:1 mix ratio
  • Recognized as meeting UL 94 HB
Product Family

3M DP100PLUS

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Epoxy
Color Color
Clear, colorless to light yellow/amber
Mix Ratio Mix Ratio
1:1
Mechanical Properties
Elongation Elongation
70 %
Physical Properties
Young's modulus Young's modulus
10.413 MPa

Leading Brands Trust in Our Products and Services