3M™ Scotch-Weld™ Structural Adhesive Film AF 3109-2U

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Structural Adhesive Film AF 3109-2U

Main features

  • High-Strength Structural Bonding
  • High- and Moderate-Tack Film Options
  • 60-Minute 250 deg F Cure

Product Description

3M™ Scotch-Weld™ Structural Adhesive Film AF 3109-2U is a thermosetting, modified epoxy structural adhesive film designed for bonding honeycomb and metal-to-metal components where high strength at 300°F (149°C) is required. The family includes high-tack, knit-scrim-supported AF 3109-2K constructions and moderate-tack, unsupported AF 3109-2U constructions, with published weights from 0.015 to 0.085 lb/ft² depending on variant. Cure temperatures range from 225°F (107°C) to 350°F (177°C), and the film is documented for metal-to-metal and honeycomb sandwich applications over a temperature range of -67°F to 300°F (-55°C to 149°C). The unsupported version can be reticulated on honeycomb.

Key features

  • High-temperature structural bonding: Designed for honeycomb and metal-to-metal bonding where high strength at 300°F (149°C) is required.
  • Supported and unsupported constructions: AF 3109-2K uses a knit-scrim carrier with high tack, while AF 3109-2U is unsupported with moderate tack.
  • Flexible heat-cure range: Published cure temperatures range from 225°F (107°C) to 350°F (177°C); a 60-minute cure at 250°F (121°C) and 40 psi is suggested when maximum results are desired.

Applications / Suitable for

  • Metal-to-metal structural bonding
  • Metal-to-honeycomb and honeycomb sandwich bonding
  • Honeycomb reticulation with the unsupported AF 3109-2U construction
Product Family

3M AF 3109-2U

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Published film construction, format, and storage information. Variant designations are preserved because carrier, tack, and film weight differ across AF 3109-2 constructions.

Property Value Unit Method / condition
Material type Thermosetting, modified epoxy adhesive film — As supplied
Color Blue — All listed AF 3109-2K and AF 3109-2U constructions
AF 3109-2K construction Knit scrim; high tack; 0.085, 0.060, 0.045 lb/ft² Published film weights; ±0.005 lb/ft²
AF 3109-2U construction Unsupported; moderate tack; 0.035, 0.015 lb/ft² Published film weights; ±0.005 lb/ft²
Recommended storage temperature 0 (-18) or below °F (°C) Recommended to obtain maximum storage life
Standard shelf life 6 months From date of shipment from 3M when stored at 0°F (-18°C) or less
Technical properties

After-processing / final-state properties

Representative or typical performance data shown for AF 3109-2K 0.085 wt. and AF 3109-2U 0.035 wt. Data were developed using EC-3960-primed aluminum and a 60-minute cure at 250°F (121°C) and 40 psi, with a 4-5°F (2-3°C)/minute rise rate. Values are not for specification purposes.

Property Value Unit Method / condition
Metal-to-metal overlap shear at 75°F (23°C) 6075 (41.9) / 5600 (38.6) psi (MPa) AF 3109-2K 0.085 wt. / AF 3109-2U 0.035 wt.; 2024-T3 alclad aluminum; 1/2 in. overlap; MMM-A-132
Metal-to-metal overlap shear at 300°F (150°C) 1740 (12.0) / 1833 (12.6) psi (MPa) AF 3109-2K 0.085 wt. / AF 3109-2U 0.035 wt.; 2024-T3 alclad aluminum; 1/2 in. overlap; MMM-A-132
Floating roller peel at 75°F (23°C) 45 (200) / 29 (129) piw (N/25 mm) AF 3109-2K 0.085 wt. / AF 3109-2U 0.035 wt.; 2024-T3 bare aluminum specimens
Honeycomb climbing drum peel at 75°F (23°C) 27.0 (120.1) / 10.3 (45.8) in·lb/in (mN/m) AF 3109-2K 0.085 wt. / AF 3109-2U 0.035 wt.; 2024-T3 bare aluminum skin with 5052 aluminum honeycomb; MIL-A-25463
Honeycomb flatwise tensile at 75°F (23°C) 1750 (12.1) / 1100 (7.6) psi (MPa) AF 3109-2K 0.085 wt. / AF 3109-2U 0.035 wt.; 2024-T3 bare aluminum skin with 5052 aluminum honeycomb; MIL-A-25463