3M 966

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

3M 966

Main features

  • Up to 232 deg C Short-Term Exposure
  • 10,000-Minute Static Shear
  • Metal and High-Energy-Plastic Bonding

Product Description

3M™ Adhesive Transfer Tape 966 is a 2.3 mil (0.06 mm) adhesive transfer tape featuring 3M™ High Temperature Acrylic Adhesive 100 on a 62# densified kraft liner. It provides excellent bonding to metals and high-surface-energy plastics, exceptional static shear performance at elevated temperatures, and resistance to demanding chemical and environmental exposure. Its low-outgassing and low-leachable-chloride characteristics make it suitable for evaluated electronic, aerospace, industrial labeling, nameplate, and die-cutting applications.

Key features

  • High-temperature performance: Supports short-term exposure up to 232°C (450°F) and long-term exposure up to 204°C (400°F).
  • Exceptional static shear: Achieves 10,000-minute static shear results at temperatures from 23 to 232°C under the published test conditions.
  • Strong high-surface-energy bonding: Provides excellent adhesion to metals and good adhesion to high-surface-energy plastics.
  • Environmental and chemical resistance: Resists humidity, water, UV exposure, temperature cycling, gasoline, oil, mild acids, and mild alkalis when properly applied.
  • Low-outgassing construction: Offers low outgassing and low leachable chloride for evaluated electronic and aerospace applications.

Applications / Suitable for

  • Bonding metal nameplates
  • High-temperature labels and identification components
  • Die-cut parts requiring a densified kraft liner
  • Evaluated electronic, aerospace, and industrial applications

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
acrylic
Release Liner Release Liner
62# Densified Kraft with “3M” printed in green
Total Thickness Total Thickness
60 μm

Additional Information

Technical properties

As-supplied / before-processing properties

Representative or typical product properties. Values should not be used for specification purposes.

Property Value Unit Method / condition
Adhesive type 3M™ High Temperature Acrylic Adhesive 100 — Pressure-sensitive acrylic adhesive
Total tape thickness 0.06 (2.3) mm (mil) ASTM D3652
Liner 62# densified kraft with “3M” printed in green — As supplied
Liner thickness 0.09 (3.6) mm (mil) Published typical value
90° peel adhesion — ABS 4.8 (44); 5.9 (54) N/cm (oz/in) ASTM D3330; 20 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min)
90° peel adhesion — stainless steel 5.8 (53); 8.5 (78) N/cm (oz/in) ASTM D3330; 20 min and 72 h dwell; 23°C (73°F); 2 mil PET backing at 20 min and 2 mil aluminum-foil backing at 72 h; 304 mm/min (12 in/min)
Static shear — 23°C (73°F) 10,000 minutes ASTM D3654; 2,000 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes
Static shear — 70°C (158°F) 10,000 minutes ASTM D3654; 1,000 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes
Static shear — 93°C (200°F) 10,000 minutes ASTM D3654; 1,000 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes
Static shear — 232°C (450°F) 10,000 minutes ASTM D3654; 400 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes
Short-term temperature resistance 232 (450) °C (°F) Short term: minutes or hours
Long-term temperature resistance 204 (400) °C (°F) Long term: days or weeks
Low-temperature service -40 (-40) °C (°F) Parts should be tested for low-temperature shock service
Thermal conductivity 0.178; 0.183; 0.187 W/m/K ASTM C518; at 41°C (107°F), 71°C (160°F), and 101°C (214°F), respectively
Dielectric constant 2.92 — ASTM D150; 23°C (73°F); 1 kHz
Dissipation factor 0.025 — ASTM D150; 23°C (73°F); 1 kHz
Dielectric strength 1,100 V/mil ASTM D149; 500 VAC RMS; 60 Hz/sec
Volume resistivity 4 × 1015 Ω·cm ASTM D257; 23°C (73°F)
Application temperature range 21 to 38 (70 to 100) °C (°F) Ideal range; application below 10°C (50°F) is not recommended for most pressure-sensitive adhesives
Shelf life 24 months From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in a sealed plastic bag and out of direct sunlight