Scotch® ATG Transfer Tape 924

Main features

  • Thin 0.002 in. (0.05 mm) profile for low-profile bonding
  • Reverse wound construction for use with ATG hand-held dispensers
  • Provides consistent and controlled adhesive application

Product Description

3M™ Scotch® ATG Tape 924 is a 0.002 in. (0.05 mm) thick adhesive transfer tape designed for reliable and efficient bonding. The tape is reverse wound on 1-inch diameter cores for smooth, controlled application using Scotch® ATG dispensers.

Product Key Features

  • Thin 0.002 in. (0.05 mm) profile for low-profile bonding
  • Reverse wound construction for use with ATG hand-held dispensers
  • Provides consistent and controlled adhesive application
  • Suitable for bonding lightweight materials
  • Enables clean, mess-free application with minimal waste
  • Designed for fast, one-handed dispensing

Applications

  • Mounting and attaching paper, cardboard, and lightweight plastics
  • Packaging and general sealing tasks
  • Point-of-purchase displays and assembly
  • Photo framing, matting, and artwork mounting
  • General office, industrial, and craft applications
Product Family

3M 924

1. Select Width
2. Select Length
3. Select Thickness
4. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Please select Width, Length, Thickness and Color.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Clear
Total Thickness Total Thickness
50 μm