3M 8992L

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 8992L

Main features

  • Linered Die-Cut Masking Format
  • High-Temperature Silicone Masking
  • Clean One-Piece Process Removal

Product Description

3M Polyester Tape 8992L is the linered version of 3M Polyester Tape 8992, combining a 0.052 mm dark-green polyester backing, silicone pressure-sensitive adhesive, and 0.075 mm polyester release liner for die cutting and converting. The tape is 0.082 mm thick excluding the liner and performs from -50 to 204 deg C. Typical data include 48 N/100 mm adhesion to steel, 998 N/100 mm tensile strength, and 148% elongation. Its thermal and chemical resistance support high-temperature masking, while the strong backing removes in one piece and leaves a sharp paint line.

Key features

  • Linered conversion format: The 0.075 mm polyester liner supports die cutting and converted masking shapes before application.
  • High-temperature silicone masking: Silicone adhesive performs from -50 to 204 deg C for powder coating and other elevated-temperature processes.
  • Strong clean process removal: High tensile strength supports one-piece removal without slivering after demanding masking operations.

Applications

Applications include high-temperature powder-coat masking, die cutting and converting, chemical milling, composite vacuum-bag holding, flash breaking, and scratch protection.

Product Family

3M 8992L

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Green
Total Thickness Total Thickness
82 μm
Mechanical Properties
Elongation Elongation
148 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
99.8 N/cm
Other Properties
Storage Temperature Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BackingPolyesterDark green
AdhesiveSiliconePressure-sensitive
Backing thickness0.052mmASTM D3652; typical
Total tape thickness0.082mmExcludes liner; ASTM D3652; typical
Liner thickness0.075mmPolyester liner; ASTM D3652; typical
Shelf life24monthsOriginal packaging; 16 to 27 deg C and 40 to 60% RH
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Adhesion to steel48N/100 mmASTM D3330; typical
Tensile strength998N/100 mmASTM D3759; typical
Elongation at break148%ASTM D3759; typical
Temperature use range-50 to 204deg COperating range