3M 8992

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 8992

Main features

  • 204 deg C Process Masking
  • Clean One-Piece Mask Removal
  • Chemical-Process Masking Resistance

Product Description

3M Polyester Tape 8992 is a dark-green polyester masking tape with pressure-sensitive silicone adhesive for high-temperature masking and process protection. The 0.082 mm tape uses a 0.052 mm polyester backing and provides typical adhesion to steel of 48 N/100 mm, tensile strength of 998 N/100 mm, and 148% elongation. The silicone adhesive performs from -50 to 204 deg C, while the polyester construction provides thermal, abrasion, and chemical resistance. The strong backing supports one-piece removal without slivering and leaves a sharp paint line after masking.

Key features

  • High-temperature silicone masking: The silicone adhesive performs from -50 to 204 deg C for demanding masking and process exposure.
  • Strong one-piece removal: A 998 N/100 mm typical tensile strength supports removal through cured coatings without slivering or breaking.
  • Chemical-process masking resistance: Polyester construction and silicone adhesive support masking in anodizing and acid or caustic chemical-milling operations.

Applications

Applications include powder-coat masking, anodizing and chemical-milling masking, composite vacuum-bag holding, flash breaking, and scratch protection during handling and shipping.

Technical Specifications

General Properties
Color Color
Dark Green
Total Thickness Total Thickness
82 μm
Mechanical Properties
Elongation Elongation
148 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
99.8 N/cm
Other Properties
Storage Temperature Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BackingPolyesterDark green
AdhesiveSiliconePressure-sensitive
Backing thickness0.052mmASTM D3652; typical
Total tape thickness0.082mmASTM D3652; typical
Shelf life24monthsOriginal packaging; 16 to 27 deg C and 40 to 60% RH
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Adhesion to steel48N/100 mmASTM D3330; typical
Tensile strength998N/100 mmASTM D3759; typical
Elongation at break148%ASTM D3759; typical
Temperature use range-50 to 204deg COperating range

Leading Brands Trust in Our Products and Services