3M 8417

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

3M 8417

Main features

  • Transparent Self-Wound Polyester Film
  • Edge-Tear-Resistant Film Backing
  • -40 to 93 deg C Exposure Range

Product Description

3M™ PET Durable Label Material 8417 is a transparent, self-wound polyester film coated with 3M™ Adhesive 100 High-temperature Acrylic. Commonly used as an overlaminate with 3M™ PET Durable Label Material 8418, it provides instant adhesion, transparency, and a tough film backing that resists edge tearing during processing and dispensing. The construction also offers documented chemical resistance and stability across elevated and low-temperature exposure conditions, supporting durable identification applications where environmental resistance is required. :contentReference[oaicite:0]{index=0}

Key features

  • Transparent overlaminate construction: Clear polyester film preserves label visibility when used as an overlaminate.
  • Durable film backing: Tough polyester resists edge tearing during processing and dispensing.
  • Environmental resistance: Documented exposure testing shows no appearance change after selected chemical, humidity, and temperature conditions.

Applications / Suitable for

  • Overlaminating 3M™ PET Durable Label Material 8418
  • Fluid-line identification
  • General identification applications requiring chemical and temperature resistance
Product Family

3M 8417

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
3M™ Adhesive 100 High-temperature Acrylic
Adhesive Thickness Adhesive Thickness
30 µm
Film Thickness Film Thickness
0.025 mm
Total Thickness Total Thickness
56 μm
Mechanical Properties
Elongation Elongation
100 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical construction, dimensional, dispensing, and storage properties of 3M™ PET Durable Label Material 8417. Values are representative and are not intended for specification purposes. :contentReference[oaicite:1]{index=1}

Property Value Unit Method / condition
Construction Self-wound transparent polyester film — Linerless construction
Adhesive type 3M™ Adhesive 100 High-temperature Acrylic — Typical construction
Total tape thickness 0.056 (2.2) mm (mil) ASTM D3652; nominal caliper
Adhesive thickness 0.03 (1.2) mm (mil) Nominal caliper
Facestock thickness 0.025 (1) mm (mil) Polyester facestock; nominal caliper
Typical unwind 3 (3) oz/in (N/100 mm) Shocky unwind
Shelf life 24 months From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in original packaging away from direct sunlight

 

Technical properties

After-processing / final-state properties

Typical adhesion, mechanical, chemical, and temperature-exposure characteristics of 3M™ PET Durable Label Material 8417. Values are representative and are not intended for specification purposes. :contentReference[oaicite:2]{index=2}

Property Value Unit Method / condition
180° peel adhesion — ABS 3.8 (35) N/cm (oz/in) ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min)
180° peel adhesion — glass 4.9 (45) N/cm (oz/in) ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min)
180° peel adhesion — polypropylene 1.2 (11) N/cm (oz/in) ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min)
180° peel adhesion — stainless steel 4.1 (38) N/cm (oz/in) ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min)
Tensile strength 43.5 (400) N/cm (oz/in) Typical
Elongation at break 100 % Typical
Chemical exposure appearance No change — 4 h immersion at room conditions; 2 × 2 in samples on stainless steel; tested with isopropyl alcohol, 10W30 oil, pH 4 acid, pH 10 base, and water; zero edge penetration
Temperature-exposure appearance No change — 24 h exposure; 2 × 2 in samples on stainless steel; tested from -40°C (-40°F) to 93°C (200°F); selected conditions also evaluated at 90% RH

Leading Brands Trust in Our Products and Services