3M™ Scotch-Weld™ Epoxy Adhesive 7260FC NS

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Epoxy Adhesive 7260FC NS

Main features

  • Toughened formulation
  • Cures at room temperature or accelerated at up to 65 °C
  • Working time of 90 minutes

Product Description

3M™ Scotch-Weld™ 7260 B/A FC-NS is a thixotropic, two-part structural epoxy adhesive developed for high-strength, toughened bonding of metals and composite materials. It is well suited for demanding industrial environments where resistance to elevated temperatures and dynamic stresses is required.

Product Key Features

  • Toughened formulation with high peel and shear strength
  • Excellent resistance to oils, water, cleaners, diesel, and similar substances
  • 90-minute working time
  • Service temperature: -55 °C to 120 °C (tested up to 200 °C)
  • Thixotropic consistency enables accurate application on vertical surfaces without sagging
  • Cures at ambient temperature or can be accelerated at temperatures up to 65 °C

Applications

  • Structural bonding of steel, aluminium, and composite materials
  • Suitable for applications exposed to thermal cycling, vibration, or impact
Product Family

3M 7260FCNS

1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Please select Package Type and Color.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Modified epoxy/modified amine
Color Color
Black/off-white
Mix Ratio Mix Ratio
2:1
Specific Gravity Specific Gravity
1.24 - 1.35
Work life @25°C Work life @25°C
1.5 hours
Physical Properties
Viscosity Viscosity
350 - 900 mPa.s