3M 70

Main features

  • Instant Self-Fusing Cable Overwrap
  • Class H High-Temperature Insulation
  • Arc-Resistant High-Voltage Protection

Product Description

Scotch Self-Fusing Silicone Rubber Electrical Tape 70 is a high-temperature, self-fusing inorganic silicone rubber tape for electrical insulation and protective overwrapping. It fuses to itself without a pressure-sensitive adhesive and uses an easy-tear, easy-strip liner for hand application. The tape provides high dielectric strength with arc and track resistance and is a Class H material for continuous operation at 180 deg C. Applied in half-lapped layers with moderate tension, it forms a fused protective wrap for high-voltage cable and other high-temperature electrical insulation work.

Key features

  • Instant self-fusion: The silicone rubber fuses to itself without a pressure-sensitive adhesive and does not need to be held down after wrapping.
  • Class H temperature capability: The 180 deg C continuous Class H rating applies to high-temperature primary insulation applications.
  • Arc and track resistance: High dielectric strength with arc and track resistance suits protective overwraps on high-voltage terminations.

Applications

Applications include high-voltage cable termination overwraps, Class H primary insulation, spacer-cable splice overwraps, and outdoor electrical protection.

Technical Specifications

General Properties
Color Color
Munsell 5BG7.0/0.4 Sky Blue Grey
Total Thickness Total Thickness
300 μm
Mechanical Properties
Elongation Elongation
450 %
Electrical Properties
Arc Resistance Arc Resistance
60 s
Dielectric Strength Dielectric Strength
34 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorSky Blue GrayMunsell 5BG7.0/0.4
Thickness0.012inTypical; ASTM D1000-10
Tensile strength12lb/inTypical; ASTM D1000-10
Elongation at break450%Typical; ASTM D1000-10
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Dielectric strength875V/milTypical; ASTM D1000-10
Arc resistance>= 1minTypical; ASTM D495-71
Continuous operating temperature180deg CClass H material