3M 69

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 69

Main features

  • High-Temperature Electrical Insulation
  • Glass-Cloth Coil and Motor Wrapping
  • No-Heat Adhesive Application

Product Description

3M Glass Cloth Electrical Tape 69 is a white, 0.178 mm electrical insulation tape with a glass-cloth backing and a non-corrosive, flame-retardant, thermosetting silicone pressure-sensitive adhesive. The adhesive applies without heat or moisture preparation, while the glass-cloth construction provides a defined tape format for high-temperature electrical assembly. The tape is designed for continuous operation not exceeding 200 deg C under its UL listing and 180 deg C under its CSA listing. Its electrical and mechanical properties suit insulation, splicing, bundling, and coil-wrapping applications where a glass-cloth tape is specified.

Key features

  • High-temperature electrical insulation: The tape is rated for continuous operation up to 200 deg C under UL and 180 deg C under CSA.
  • Glass-cloth silicone construction: A 0.140 mm glass-cloth backing with thermosetting silicone adhesive provides a 0.178 mm insulation tape.
  • Ready pressure-sensitive application: The adhesive applies without heat or moisture preparation for coil, transformer, and motor assembly.

Applications

It is used for coil, transformer, and motor insulation, lead anchoring, high-temperature electrical splicing, and bundling.

Product Family

3M 69

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
White
Total Thickness Total Thickness
177 μm
Other Properties
Storage Temperature Storage Temperature
10 - 27 °C
Mechanical Properties
Elongation Elongation
5 %
Thermal Properties
Operating Temperature Operating Temperature
200 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorWhiteVisual
Backing materialGlass clothAs supplied
Backing thickness0.140mmNominal
Total thickness0.178 +/- 0.025mmASTM D1000; 23 deg C
AdhesiveThermosetting siliconePressure-sensitive
Breaking strength>= 263N/cmMinimum; ASTM D1000; 23 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Dielectric breakdown>= 2000VMinimum; ASTM D1000; 23 deg C
Insulation resistance>= 50 x 10^6ohmMinimum; ASTM D1000 high-humidity method
Adhesion to steel>= 3.3N/cmMinimum; ASTM D1000; 23 deg C
UL continuous operating temperature200deg CDo not exceed; UL listing
CSA continuous operating temperature180deg CDo not exceed; CSA listing