3M 4200FC

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 4200FC

Main features

  • Fast Moisture-Cure Sealing
  • Non-Sag Marine Application
  • Flexible Bonds for Disassembly

Product Description

3M Marine Adhesive Sealant Fast Cure 4200FC is a one-part, moisture-curing polyurethane paste for bonding and sealing marine joints and hardware. Its medium-strength elastomeric seal is watertight and weather resistant while allowing later disassembly. At 73 deg F and 50% relative humidity, the typical tack-free time is 1 to 2 hours and the typical cure rate is 4 mm per 24 hours. The sealant can be used with wood, fiberglass, gelcoat, selected plastics, and metals; some plastics require testing and metals may require primer. It is used above and below the waterline on deck-to-hull joints, portholes, deck fittings, rub rails, screw holes, and stanchion supports.

Key features

  • Fast Moisture Cure: Forms a tack-free surface in a typical 1 to 2 hours at 73 deg F and 50% relative humidity.
  • Flexible Disassemblable Seal: The medium-strength elastomeric bond remains flexible and permits later disassembly.
  • Non-Sag Marine Application: The caulkable paste stays non-sagging for marine joints and hardware above or below the waterline.

Applications

Suitable for fiberglass deck-to-hull joints, wood-to-fiberglass bonding, portholes, deck fittings, rub-rail attachment, screw holes, and stanchion supports.

Technical Specifications

General Properties
Color Color
White, Black
Density (g) Density (g)
1.2 g/cm3
Solids Solids
100 %
Physical Properties
Tack-Free Time Tack-Free Time
60 - 120 minutes
Mechanical Properties
Elongation Elongation
>400 %
Other Properties
Storage Temperature Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Technical values are representative or typical and are not specifications.

PropertyValueUnitMethod / condition
ConsistencyCaulkable, non-sag paste-Typical; as supplied
Density9.75lb/galApproximate; typical
Solids content100%Approximate; typical
Tack-free time1 to 2hoursTypical at 73 deg F (23 deg C) and 50% RH
Rate of cure3/16 (4)in (mm) per 24 hTypical at 73 deg F (23 deg C) and 50% RH
Application surface temperature40 to 100 (4 to 38)deg F (deg C)Do not apply to frost-covered surfaces
Technical properties

Final-state / after-processing properties

Technical values are representative or typical and are not specifications.

PropertyValueUnitMethod / condition
Shore A hardness40-Typical; ASTM C661
Tensile strength180 (1.24)psi (MPa)Typical; ASTM D412
Elongation at break>400%Typical; ASTM D412
Service temperature-40 to 190 (-40 to 88)deg F (deg C)Typical product data