3M 40PR

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 40PR

Main features

  • Conductive Anti-Static Adhesion
  • Visible Static-Control Identification
  • 130 deg C Process Exposure

Product Description

3M Anti-Static Electronic Tape 40PR is a 0.055 mm (2.2 mil) polyester utility tape with an anti-static conductive-polymer acrylic adhesive for static-sensitive manufacturing areas. The 0.025 mm (1 mil) backing is preprinted with a static symbol for immediate visual identification during masking, holding, and process protection. Firm adhesion keeps the tape positioned while its anti-static construction is designed to reduce ESD risk to sensitive electronic equipment. The applied tape withstands temperatures up to 130 deg C (266 deg F) and complies with RoHS 2011/65/EU. It suits electronics assembly, clean work areas, and other production steps that require visible anti-static tape control.

Key features

  • Anti-Static Conductive Adhesive: The conductive-polymer acrylic adhesive combines firm holding with static-control performance.
  • Printed Static Identification: A preprinted static symbol makes the tape easy to identify in sensitive work areas.
  • 130 deg C Temperature Capability: The applied tape withstands temperatures up to 130 deg C (266 deg F).

Applications

Suitable for masking, holding, packaging, and process protection in static-sensitive electronics manufacturing and clean work areas.

Product Family

3M 40PR

Loading pricing…

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BackingPolyester film-Anti-static
Backing thickness0.025 (1)mm (mil)As supplied
Total thickness0.055 (2.2)mm (mil)As supplied
AdhesiveConductive-polymer acrylic-Anti-static
Printed markingStatic symbol-As supplied
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Maximum operating temperature130 (266)deg C (deg F)Applied tape
AdherenceFirm-Applied tape
ESD functionDesigned to prevent ESD damage-Sensitive electronic equipment
ComplianceRoHS 2011/65/EU-Product construction