3M 3901

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 3901

Main features

  • Low-Viscosity Surface Wetting
  • Quick-Drying One-Component Application
  • Improved Metal Corrosion Protection

Product Description

3M Scotch-Weld Metal Primer 3901 is a red, low-viscosity, one-component liquid primer for preparing metal and glass before bonding with compatible 3M Scotch-Weld film and liquid structural adhesives. It wets treated surfaces thoroughly and dries quickly, simplifying application before adhesive placement. The primer helps maintain cleaned surfaces in a relatively oxidation-free condition until bonding is completed. In the bonded interface, it improves adhesion and resistance to environmental exposure while adding corrosion protection on metal. The 3 to 8 cP viscosity supports thin, even coverage for glass and metal assemblies that require controlled primer application and dependable structural-adhesive preparation.

Key features

  • Low-Viscosity Surface Wetting: The 3 to 8 cP liquid spreads readily for complete wetting before adhesive placement.
  • Quick-Drying One-Component Application: The ready-to-use primer simplifies surface preparation without component mixing.
  • Metal Corrosion Protection: The dried primer improves resistance to corrosion and environmental exposure on metal.

Applications

Suitable for priming metal and glass before compatible 3M Scotch-Weld film and liquid structural adhesives.

Technical Specifications

General Properties
Color Color
Red
Physical Properties
Viscosity Viscosity
5 ± 2 mPa.s
Other Properties
Storage Temperature Storage Temperature
16 -27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Physical stateLiquid-As supplied
ColorRed-As supplied
Viscosity3 to 8cPAs supplied
Density0.80g/mlAs supplied
Flash point52deg FClosed cup
Boiling point148deg FAs supplied
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Adhesion functionImproves metal and glass adhesion-Compatible 3M film and liquid structural adhesives
Corrosion protectionImproved-Metal surfaces
Environmental-exposure resistanceImproved-Primed metal interface
Cleaned-surface protectionMaintains relatively oxidation-free condition-Until bonding is completed