3M 3747

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M 3747

Main features

  • Dissimilar-Substrate Hot-Melt Bonding
  • Rapid Strength Development in Seconds
  • 45-Second Open Time

Product Description

3M™ Hot Melt Adhesive 3747 is a 100% solids, thermoplastic general-purpose adhesive designed for bonding dissimilar substrates. Containing no VOCs, this tan-colored hot melt adhesive applies easily and sets in seconds without the need for clamping. It provides an open time of 45 seconds and is highly effective for a wide variety of assemblies, including joining wood to plastic and fabric to metal.

Key features

  • Fast setting time: Adhesive sets and obtains high-performance strength in seconds, eliminating the need for clamping.
  • Versatile bonding: General-purpose formulation easily bonds dissimilar substrates such as wood to plastic and fabric to metal.
  • Easy to use: 100% solids, VOC-free formula provides a 45-second open time for easy handling on large assemblies and surfaces.

Applications / Suitable for

  • Woodworking applications
  • General industrial bonding
  • Bonding dissimilar substrates like wood to plastic and fabric to metal

Technical Specifications

General Properties
Color Color
Tan
Density (g) Density (g)
0.97 g/cm3
Thermal Properties
Flash Point Flash Point
509 °C
Physical Properties
Open time Open time
<1 (45 seconds) minutes
Viscosity Viscosity
4,100 mPa.s
Mechanical Properties
Peel Strength Peel Strength
20 piw
Physical Properties
Softening point (Melting point) Softening point (Melting point)
104 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Color Tan - Solid
Density 0.97 g/cm³ -
Viscosity 4,100 cP at 375°F
Flash Point 509 °F Cleveland Open Cup ASTM D 92-72
Open Time 45 seconds 1/8" bead on non-metallic substrates at 75°F
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Shear Strength 430 psi Overlap shear measured on Douglas Fir to Douglas Fir
Peel Strength 20 piw Flexible canvas bonded to Douglas Fir
Heat Resistance 145 °F Highest temperature supporting a 2 psi dead load (63°C)
Ball & Ring Melt Point 220 °F ASTM E28-67 (104°C)