Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 218

Main features

  • Crisp Fine-Line Separation
  • Solvent and Moisture Resistance
  • Bake-Cycle Heat Resistance

Product Description

Scotch Fine Line Tape 218 is a green polypropylene-film fine-line masking tape for producing crisp paint edges on straight lines and sweeping curves. Its natural-rubber pressure-sensitive adhesive provides high instant adhesion, while the low-profile backing supports color separation and conforms around corners. The tape resists most solvents and moisture and withstands bake cycles up to 121 deg C for 30 minutes. Typical construction values include 0.13 mm total thickness, 720% elongation at break, and 22.8 N/cm tensile strength. It is used for fine-line masking in specialty vehicle, automotive, rail, marine, aerospace, two-tone, multicolor, and custom graphic finishing.

Key features

  • Crisp color separation: The low-profile backing and high adhesion support sharp paint lines on straight and sweeping layouts.
  • Solvent and moisture resistance: The tape resists most solvents and moisture during supported paint-finishing work.
  • Bake-cycle capability: The applied tape withstands bake cycles up to 121 deg C for 30 minutes.

Applications

Applications include fine-line paint masking, two-tone and multicolor layouts, custom graphics, and specialty vehicle, automotive, rail, marine, and aerospace finishing.

Technical Specifications

General Properties
Color Color
Green, matte finish
Mechanical Properties
Elongation Elongation
720 %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
22.8 N/cm
Other Properties
Storage Temperature Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorGreen-Typical
BackingPolypropylene film-As supplied
AdhesiveRubber-Pressure-sensitive
Total thickness5 (0.13)mil (mm)Typical
Elongation at break720%Typical
Tensile strength13 (22.8)lb/in (N/cm)Typical
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Bake-cycle heat resistance121 (250)deg C (deg F)Up to 30 min
Clean removalYes-Applied tape
Solvent resistanceResistant to most solvents-Applied tape
Moisture resistanceResistant-Applied tape