3M 2158

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 2158

Main features

  • High-Strength Structural Bonding
  • 120-Minute Working Window
  • 1:1 Meter-Mix Processing

Product Description

3M™ Scotch-Weld™ Epoxy Adhesive 2158 B/A is a two-part, high-strength epoxy adhesive that chemically cures at room temperature to form a durable gray bond. It provides excellent adhesion to a wide variety of substrates, including metals, many plastics, wood, and damp concrete. Featuring a convenient 1:1 mix ratio by weight or volume, it is also recognized as meeting UL 94 HB standards for flammability.

Key features

  • Convenient mix ratio: Features a 1:1 mix ratio by weight or volume for simplified dispensing and application.
  • Versatile adhesion: Bonds strongly to multiple substrates, including metals, plastics, wood, and damp concrete.
  • Extended work life: Offers a 120-minute open time at room temperature, allowing ample time for complex assemblies and positioning.

Applications / Suitable for

  • High-strength structural bonding
  • Assembling metals, plastics, and wood
  • Applications requiring bonding to damp concrete

Technical Specifications

General Properties
Mix Ratio Mix Ratio
1:1
Solids Solids
100 %
Work life @25°C Work life @25°C
2 hours
Physical Properties
Viscosity (Part A) Viscosity (Part A)
200,000 - 800,000 mPa.s
Viscosity (Part B) Viscosity (Part B)
250,000 - 450,000 mPa.s
Mechanical Properties
Elongation Elongation
54 %
Peel Strength Peel Strength
3 lb/in width
Electrical Properties
Volume Resistivity Volume Resistivity
1.4E+15 Ohms⋅cm
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
52 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Mix Ratio 1:1 - By weight or volume
Color White - Base
Color Dark Gray - Accelerator
Viscosity 250,000 - 450,000 cP Base at 23°C
Viscosity 200,000 - 800,000 cP Accelerator at 23°C
Work Life 120 minutes 100g mixed at 23°C
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Cured Color Gray - -
Durometer Hardness 85 Shore D ASTM D2240
T-Peel Adhesion 3 lb/in width ASTM D1876, FPL Etched Aluminum
Dielectric Constant 5.6 - 1 KHz (ASTM D150)
Volume Resistivity 1.4E+15 Ohm-cm ASTM D257

Leading Brands Trust in Our Products and Services