3M™ Fastbond™ 2000NF

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Fastbond™ 2000NF

Main features

  • Quick bonding without heat
  • Immediate handling strength.
  • Post-formable and heat resistant

Product Description

3M™ Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a waterdispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced drying equipment for most applications.

Product Key Features

  • Quick bonding without heat
  • Immediate handling strength
  • Bonds flexible polyurethane and latex foams, plastic laminate, wood, plywood, particle board, fabrics, fiber, aluminum, galvanized steel and many plastics
  • Designed to be applied between two substrates

Applications

 

  • Furniture & Seating: Attaching foam cushions and upholstery fabrics to wood, metal, or plastic frames.
  • Cabinetry & Woodworking: Laminating high-pressure plastics (HPL) to countertops, MDF, or plywood.
  • Acoustic & Wall Panels: Adhering fiberglass insulation, fabrics, and acoustic foam to partitions.
  • Transportation Interiors: Assembling headliners, trim, and seating in aerospace, marine, and RV industries.

 

Product Family

3M 2000NF

1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Please select Package Type and Color.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Polychloroprene
Color Color
Blue, Light Orange or Neutral
Solids Solids
47-51 %
Physical Properties
Viscosity Viscosity
200-750 mPa.s