3M 1267

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 1267

Main features

  • Embossed Z-Axis Contact
  • 64 dB Average Shielding
  • Lined Die-Cut Handling

Product Description

3M Embossed Aluminum EMI Shielding Tape 1267 uses a 2.0 mil embossed, dead-soft aluminum backing coated with non-conductive acrylic adhesive in a 4.95 mil tape for grounding and EMI control. During installation, raised foil edges penetrate the adhesive and establish z-axis contact with the substrate; conductivity does not come from the adhesive itself. ASTM D4935 testing gives 64 dB average shielding effectiveness across 300 kHz to 2.5 GHz, while the stated MIL-STD-202 method limits electrical resistance to 0.0075 ohm/in2 maximum. A removable liner aids die-cut conversion and controlled placement in equipment, components, shielded rooms, and prototype assemblies.

Key features

  • Embossed contact path: The aluminum embossing penetrates the non-conductive adhesive to establish foil-to-substrate electrical contact.
  • Measured shielding performance: Average shielding effectiveness is 64 dB from 300 kHz to 2.5 GHz under ASTM D4935.
  • Lined die-cut handling: The removable liner supports converting, die cutting, placement, and prototype work.

Applications

Applications include grounding and EMI shielding in equipment, components, and shielded rooms, plus die-cut parts, electrical prototyping, design work, and troubleshooting.

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
non-conductive acrylic
Color Color
silver
Film Thickness Film Thickness
0.051 mm
Total Thickness Total Thickness
4.96 μm
Mechanical Properties
Adhesion Strength Adhesion Strength
30.2 Oz/in

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorSilver-Visual
BackingEmbossed aluminum foil-As supplied
AdhesiveNon-conductive acrylic-Non-corrosive pressure-sensitive adhesive
Backing thickness2.0 / 0.051mil / mmNominal
Total thickness4.95 +/- 0.65 / 0.126mil / mmASTM D1000 at 23 deg C
Shelf life5yearsFrom manufacture; 10 to 27 deg C and less than 75% RH
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Electrical resistance0.0075ohm/in2Maximum; MIL-STD-202 Method 307 at 5 psi over 1 in2
Shielding effectiveness64dBAverage; ASTM D4935, 300 kHz to 2.5 GHz at 23 deg C
Adhesion to steel30.2 / 3.3oz/in / N/cmMinimum; ASTM D1000 at 23 deg C
Breaking strength14 / 25lb/in / N/cmMinimum; ASTM D1000 at 23 deg C
Flame retardancyPass-UL 510A, Category OARC2, File E17385