3M 1218

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 1218

Main features

  • 180 deg C Continuous Operation
  • Thin High-Temperature Insulation
  • Flexible-Circuit Cover Layer

Product Description

3M Polyimide Film Electrical Tape 1218 combines a 0.025 mm polyimide film backing with a non-corrosive acrylic PSA in a 0.080 mm tape for high-temperature electrical insulation. Rated under its UL listing for continuous operation up to 180 deg C, it provides minimum dielectric breakdown of 5500 V; insulation resistance is at least 1 x 10^12 ohm by ASTM D1000 at 23 deg C. The amber tape wraps coils, capacitors, transformers, wire harnesses, and leads, and also serves as a cover layer for flexible printed circuits or a solder mask during printed circuit board assembly.

Key features

  • 180 deg C operation: The tape is designed for continuous operation not exceeding 180 deg C under its UL listing.
  • Thin insulation profile: The construction combines 0.025 mm polyimide backing with 0.080 mm total tape thickness.
  • No-preparation adhesive: The acrylic pressure-sensitive adhesive requires no heat, moisture, or solvent preparation for application.

Applications

Applications include wrapping coils, capacitors, transformers, wire harnesses, and leads; solder masking; and cover-layer use on flexible printed circuits.

Product Family

3M 1218

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
Pressure Sensitive Acrylic
Total Thickness Total Thickness
76 μm
Thermal Properties
Operating Temperature Operating Temperature
180 °C
Mechanical Properties
Adhesion Strength Adhesion Strength
19 Oz/in
Elongation Elongation
55 %
Electrical Properties
Breakdown Voltage Breakdown Voltage
6,000 V

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorAmber-Visual
BackingPolyimide film-As supplied
AdhesiveAcrylic-Non-corrosive pressure-sensitive adhesive
Backing thickness1 / 0.025mil / mmNominal
Total thickness3.15 +/- 0.2 / 0.080 +/- 0.005mil / mmASTM D1000 at 23 deg C
Shelf life5yearsFrom manufacture; 10 to 27 deg C and less than 75% RH
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Continuous operating temperature180deg CMaximum under UL listing
Dielectric breakdown5500VMinimum; ASTM D1000 at 23 deg C
Insulation resistance1 x 10^12ohmMinimum; ASTM D1000 at 23 deg C
Electrolytic corrosion factor1.0-3M ETM-54001; 1.0 equals no observed corrosion
Adhesion to steel14 / 1.5oz/in / N/cmMinimum; ASTM D1000 at 23 deg C
Breaking strength20 / 35lb/in / N/cmMinimum; ASTM D1000 at 23 deg C
Elongation50%Minimum; ASTM D1000 at 23 deg C
Flame retardancyPass-UL 510A

Leading Brands Trust in Our Products and Services